Increase to quotation Only exhibit this consumer #8 · Nov 29, 2020 Alliant has a tendency to publish facts largely showing the exact same firms hulls and primers. I contacted them a couple of load demonstrating only Fed 209a primers (strain was 8200) and inquire if I could substitute a Earn 209 or CCI 209M and so they responded expressing no issue Together with the primer substitution. Velocity will most likely be reduced with possibly of such, given that as said higher than the Fed 209a is hotter.

So in conclusion, you'll be able to securely use that Fed 209 primer in just about every recipe that lists Fed 209 A primers, so long as you assume much less velocity and less strain as part of your hundreds.

shot, TiteWad powder, Claybuster CB0175-12 wads and Here's a breakdown on the primers. The information is from Claybuster. There are several Many others but I try out to remain under 8000 psi.

The one thing that matters is tension and darn couple men and women will spend the money to amass the tools To do that but if you are doing, that really (evidently) essential velocity will probably be attained (and properly).

Base line is that they DO Without a doubt Have got a genuine location in The complete plan of matters, if Employed in the appropriate element combos.

I could find wsf load in twenty ga in any respect.I think i was not using the guide correctly . It is the only manual i have at any time witnessed that didn't have each individual component within a load on precisely the same horizonal line.I'll look it up online and may Federal 209A well go back and have the WSF if it is a good in good shape for twenty Ga seven/eight ozs

I nonetheless Possess a couple of thousand 12C1 wads, but have applied the Spolar Gold Windjammer with great results also.

If this question associated 12 ga., I'd personally say no problem. Nevertheless it's twenty ga. and items take place way Federal 209A more immediately While using the scaled-down gauges. I don't know the number of Fed primers you have but if its sufficient, I'd personally deliver a couple of samples off for being examined.

I've applied up all the outdated Fed 209 primers that I experienced, but when I was loading them I simply used them in recipes that referred to as for that W209 primer.

You will discover presently 209 muzzleloader primers in inventory which are specially intended for inline muzzleloader gun fanatics. They are really routinely analyzed and deliver exceptional success every time you shoot.

This recipe promises 1200fps at 8200psi While using the Win209 and 1200fps at 8700psi Together with the Fed209. I am able to substitute these primers with no problem. I only load known analyzed recipes and cargo while in the mid number of them to allow for any weighty drop or Various other fluke which will (and will) at some point take place. Click on to grow...

5 to one.0 grain when subbing the federal 209A for my normal Cheddite or Gain. 209. But, I always run average hundreds that are well below max Federal 209A pressure. Comply with Curly's suggestions and try to search out a published recipe on your parts. 1 position you could try could be the reloading information Middle at Hodgdon. They publish masses for IMR in addition and could have Everything you are searching for.